Structure and Tribotechnical Characteristics of NiAl–CrB2 Composite Materials and Coatings

  
M.S.Ukrainets,
 
L.M.Kapitanchuk
 

I. M. Frantsevich Institute for Problems of Materials Science of the NAS of Ukraine, Omeliana Pritsaka str.,3, Kyiv, 03142, Ukraine
Powder Metallurgy - Kiev: Frantsevich Institute for Problems of Materials Science NASU, 2015, #01/02
http://www.materials.kiev.ua/article/1890

Abstract

The influence of chromium diboride additions on the tribotechnical characteristics of NiAl–CrB2 composite coatings in friction against a counterface made of NiAl plasma-sprayed coating is studied. The friction surfaces of the plasma-sprayed composite NiAl coatings with different chromium diboride contents (5, 15, and 30 wt.%) are examined. It is established that wear substantially depends on the amount of refractory component.


CHROMIUM BORIDE, COMPOSITION COATINGS, HIGH-TEMPERATURE TRIBOLOGICAL TESTS, NIAL INTERMETALLIC, WEAR RESISTANCE